News

Micro-Arc Oxidation Technology for Magnesium Alloys

Abstract:
Magnesium alloys, known for their abundant reserves on Earth and exceptional lightweight properties, have garnered significant attention in various engineering applications. However, their inherent susceptibility to corrosion necessitates advanced surface treatment techniques. This paper introduces magnesium alloys, their characteristics, and prevalent surface treatment methods, with a focus on micro-arc oxidation (MAO) technology. MAO, an innovative technique that forms a ceramic coating in-situ on the alloy surface, significantly enhances corrosion resistance and provides additional functional properties. The paper elaborates on the fundamentals of MAO, including process principles, pretreatment and post-treatment steps, and discusses its potential applications in automotive, aerospace, electronics, and other industries.

Keywords: Magnesium alloys, micro-arc oxidation, corrosion resistance, surface treatment, ceramic coating

1. Introduction to Magnesium Alloys

Magnesium, one of the most abundant elements on Earth, comprises 2.3% of the Earth's crust in metallic minerals. As a lightweight metal with a silvery-white appearance, pure magnesium boasts a melting point of 651°C and a density ranging from 1.75 to 1.85 g/cm³, approximately one-fourth that of steel and two-thirds that of aluminum. Despite its low density, pure magnesium exhibits poor mechanical properties, limiting its direct use as a structural material. However, through alloying and heat treatment, the strength of magnesium alloys is significantly improved, leading to their widespread adoption.

 

The designation of magnesium alloys typically comprises two alphabetic characters followed by two numbers. The letters represent the primary alloying elements, while the numbers indicate the mass fractions of these elements. For instance, AZ91 signifies a magnesium alloy containing approximately 9% aluminum and 1% zinc.

Common Magnesium Alloys Include:

MB8: Al 0.2%, Mn 1.3-2.2%, Zn 0.3%, Ce 0.15-0.35%, Ni 0.07%, Si 0.1%, impurities 0.3%, balance Mg.

AZ91D: Al 8.3-9.7%, Zn 0.35-1.0%, Mn 0.15-0.5%, Si 0.1%, Cu 0.03%, Ni 0.002%, Fe 0.005%, other impurities 0.02%, balance Mg.

2. Characteristics of Magnesium Alloys

Magnesium alloys exhibit several desirable properties, including excellent machinability, high impact and compressive strength, superior damping and shock absorption capabilities, good electrical and thermal conductivity, excellent electromagnetic shielding properties, and dimensional stability. Furthermore, they are environmentally friendly, posing no pollution concerns. These attributes have led to their extensive applications in automotive, motorcycle, and aircraft components, as well as in aerospace, electronics, military, nuclear energy, computers, and communication devices.

 

3. Surface Treatment Technologies

Due to their low electrode potential, magnesium alloys are highly prone to corrosion. While they naturally form an alkaline carbonate film in the atmosphere, this film is insufficient to protect against corrosion in harsh environments. Consequently, reliable surface protection measures are necessary to enhance their corrosion resistance when used as structural materials or housings.

Current surface treatment technologies for magnesium alloys encompass chemical conversion coatings, anodizing, electroplating, micro-arc oxidation (MAO), laser treatment, cold spray, and plasma immersion ion implantation. Each technique has its unique advantages and application scenarios.

 

4. Micro-Arc Oxidation (MAO) Technology

MAO is an advanced surface treatment technique that employs electrochemical methods to generate sparks on the alloy surface immersed in an electrolyte solution. This process, occurring under the combined effects of thermochemistry, plasma chemistry, and electrochemistry, results in the in-situ growth of a ceramic coating on the alloy.

During MAO, compressed air or propellers are used to stir the electrolyte, ensuring uniform concentration and temperature. Additionally, a cooling water jacket made of stainless steel or plastic is employed to maintain a moderate electrolyte temperature.

5. MAO Surface Treatment Process

The MAO process comprises three major stages: pre-treatment, MAO treatment, and post-treatment.

Pre-treatment Stage: Compared to other magnesium alloy surface treatment technologies, the pre-treatment for micro-arc oxidation is relatively straightforward, comprising two primary steps: degreasing and cleaning. Degreasing involves using alkaline solutions, electrolysis, ultrasonic waves, or other methods to remove oil, grease, dust, iron filings, and other impurities adhered to the surface of the magnesium alloy substrate.

Cleaning follows the degreasing process, typically involving rinsing the magnesium alloy surface with clean water to wash away residual contaminants, eliminate unnecessary surface components, and enhance the quality of the subsequent micro-arc oxidation treatment.

Micro-arc Oxidation Stage: The pre-treated magnesium alloy is immersed in the micro-arc oxidation solution, and the cathode is connected. The power supply of the equipment is then turned on to initiate the micro-arc oxidation process. The crux of this stage lies in determining the optimal parameters for the micro-arc oxidation technology through extensive experimentation, data analysis, continuous testing, debugging, and refinement, based on the understanding of how various parameters affect the micro-arc ceramic layer.

Post-treatment Stage: Due to the presence of numerous micro-pores on the surface of the micro-arc oxidized ceramic layer, sealing these pores is essential to further improve the corrosion resistance of the layer. Sealing not only enhances the corrosion resistance of the micro-arc ceramic layer but also enhances its color, texture, and overall aesthetics. Common sealing agents include deionized water, paraffin, acrylic acid, epoxy resin, or phenolic varnish. Deionized water sealing involves immersing the micro-arc anodized magnesium alloy in boiling water for approximately 10 minutes. For organic sealing, the epoxy resin or phenolic varnish is diluted with acetone, and the micro-arc anodized magnesium alloy is repeatedly dipped into the organic solution and then allowed to dry.