News
Selection Method for Die Casting Machine Parameters
Abstract:
The selection of die casting machine tonnage is crucial for efficient utilization of equipment capabilities. This process is integral to both the initial quoting of die casting products and the design of die casting molds. This paper outlines a three-step approach for determining the appropriate die casting machine tonnage, focusing on the verification of clamping force, mold filling percentage, and mold dimension compatibility. Furthermore, it analyzes the injection process of horizontal cold chamber die casting machines, including pressure and velocity profiles, and discusses key pressure parameters such as injection force, specific pressure, bulging force, and clamping force, providing recommendations for optimizing casting quality.
Keywords: Die casting machine, tonnage selection, clamping force, mold filling percentage, pressure parameters, bulging force
The calculation of the required tonnage for die casting equipment is crucial for efficiently utilizing the machine's capabilities. This process is integral during the initial stages of die casting product quotation and in the design phase of die casting molds.
Figure 1: Schematic Diagram of Die Casting Machine Structure
I. Selection of Tonnage Based on Three Steps
- Verification of Clamping Force
1.1 Calculate the total projected area (A):
A=A1+A2(0.15∼0.3A1)+A3(0.1∼0.2A1)+A4(πd2)
where A1 is the projected area of the casting, A2 is the runner area, A3 is the overflow system area, A4 is the sprue area (d is the diameter of the shot sleeve, also known as the plunger diameter).
1.2 Determine the bulging force (F1):
F1=A×Injection Pressure (MPa)
The injection pressure varies based on the type of casting: 30~50 MPa for general parts, 50~80 MPa for load-bearing parts, and 80~100 MPa for gas-tight parts.
1.3 Calculate the clamping force (F2):
F2=KF1
where K is the safety factor, typically 0.85.
Initially select a die casting machine based on the calculated clamping force.
- Verification of Mold Filling Percentage
2.1 Calculate the total weight of the casting, runners, sprue, and overflow system. With the projected areas and depths known, the volumes can be determined.
2.2 Calculate the filling percentage:
Filling Percentage=Shot WeightTotal Weight
The shot weight is the maximum alloy weight for the shot sleeve of different die casting machines. Adjust the initial machine selection based on a filling percentage typically between 40% and 75%.
- Verification of Mold Dimensions
3.1 Conduct a simple mold layout for the casting to determine the mold dimensions.
3.2 Verify the suitability of the selected die casting machine's tie bar spacing based on the mold dimensions.
II. Determination of Die Casting Machine Tonnage
For analytical purposes, Figures 1 and 2 illustrate the injection process and curve of a horizontal cold chamber die casting machine. The injection process is analyzed in three stages:
Stage 1: Consists of 0-I and I-II segments. In 0-I, the plunger moves slowly to seal the pouring gate and push the metal upward smoothly. In I-II, the plunger accelerates to fill the front end of the shot sleeve.
Stage 2: II-III segment, where the plunger moves rapidly to fill the entire mold cavity and gating system.
Stage 3: III-IV segment, the final pressing stage where the plunger motion nearly stops, with the velocity gradually decreasing to zero.

Figure 2: Diagram of injection process of horizontal cold chamber die casting machine

Figure3: Pressure Injection Curve of Horizontal Cold Chamber Die Casting Machine
III. Equipment Pressure Parameters
- Injection Pressure
During the 0-I stage, the injection force is used to overcome the frictional resistance between the injection chamber and the injection plunger, as well as between the hydraulic cylinder and the piston.
In the I-II stage, the injection pressure increases, generating the first pressure peak, sufficient to overcome the resistance of the ingate.
From II-III, the injection pressure continues to rise, resulting in the second pressure peak.
In the III-IV stage, the injection force acts on the solidifying metal, compacting it. This stage requires an intensification mechanism, and the force at this stage is also known as intensification injection pressure.
- Pressure Ratio
Pressure ratio can be divided into injection pressure ratio and intensification pressure ratio.
During the 0-III stage of the injection motion, the injection pressure per unit area of metal liquid in the injection chamber is called the injection pressure ratio.
In the III-IV stage, the intensification injection pressure per unit area of metal liquid in the injection chamber is referred to as the intensification pressure ratio. The pressure ratio is one of the critical parameters ensuring casting quality. Recommended intensification pressure ratios are listed in the following table.
- Swelling Force
During die casting, the force transmitted by the metal liquid filling the cavity to the cavity wall of the mold through the pressure of the injection piston is called the swelling force.
The main swelling force (F_main) is equal to the projected area of the casting on the parting surface (or the sum of the projected areas for a multi-cavity mold), plus the area of the gating system, overflow, and venting system (typically 30% of the total area), multiplied by the pressure ratio. The calculation formula is:
Fmain=10A×Pb
where Fmain is the main swelling force (KN); A is the projected area of the casting on the parting surface (cm²); Pb is the injection pressure ratio (MPa).
The partial swelling force ((F_{\text{partial}})) is the sum of the swelling forces caused by the component forces acting on the inclined pin ejection, inclined slide ejection, and hydraulic ejection locking surfaces.
- Clamping Force
The clamping force is the most fundamental parameter indicating the size of the die casting machine, and its role is to overcome the swelling force during die filling. In die casting production, it is essential to ensure that the mold does not expand under the influence of the swelling force. The clamping force of the die casting machine must be greater than the swelling force to ensure reliability. The relationship between clamping force and swelling force is as follows:
Fclamp≥K×(Fmain+Fpartial)
where Fclamp is the clamping force required by the die casting machine (KN); K is the safety factor, typically taken as 1.25; Fmain is the main swelling force (KN); Fpartial is the partial swelling force (KN).
During die casting production, the selection of clamping force directly affects factors such as splashing of molten metal at the parting surface, the density of internal structures in castings, the presence of porosity, the completeness of forming, and the occurrence of flash and burrs. When adjusting, the clamping force should be minimized as much as possible while ensuring the quality of the castings.
Conclusion
The selection of the right die casting machine tonnage is a critical step in ensuring the success of a die casting project. By considering factors such as casting dimensions, material properties, injection pressure, mold design, and safety margins, engineers can make informed decisions that optimize machine performance, improve casting quality, and reduce production costs. The methodology outlined in this paper provides a practical framework for selecting the appropriate die casting machine tonnage during the product quotation and mold design phases